I'll try to answer all your questions, Burnhard.
One of the reasons it's hard for the layperson to determine prices for sodium cyanide is that it is a regulated commodity. Its toxic characteristics limit access to those who have a real need for the chemical in their businesses. As a chemist myself, I know where to look. A decade ago, sodium cyanide went for $0.50-.55 per pound, if bought in bulk. Recent quotations are roughly $1/lb., but I've seen it for a little less, by the container load. Potassium cyanide is maybe five times as expensive. Occasionally, calcium cyanide is used to extract gold from ore, but I didn't price it. Sodium cyanide is, by far, the most commonly form of cyanide used.
There are two distinct applications for cyanidation of gold ore. The more cost-effective for high-tonnage low-grade deposits is employing a heap leach pad. An impermeable base is prepared, with drainage channels built in. Then crushed ore is heaped on top. Cyanide solution is sprayed onto the heap, and the gold (and silver and copper, if any) is dissolved by the cyanide solution, which is collected at the base of the leach pad. Then there are a variety of methods to free the gold and other metals from solution. I was just reading about a plan by Couer D'Allene to build a 200 million tonne pad in Nevada, at their Rochester project (potentially complicated by their failure to pay the BLM fees, letting some claims drop, which were scooped up by Ryepatch, but that's another issue). Now get this, the estimated grade of the ore is 0.3 gpt gold, and between 6 and 10 gpt silver. And yet, they think it economic to build this massive heap leach system. It will take six years to build it, and up to 20 years to leach the precious metals to the point where it is no longer economic to continue.
Another approach is to expose crushed ore to an excess of cyanide solution in large tanks. The powdered ore is stirred up and quick-leached (compared to the heap leach method). The dwell time (the actual time the ore is exposed to the cyanide solution) is closely controlled, as there is an optimum period of maximal recovery, while minimizing processing time (and thus costs). UC has this type of system at La Yesca. I believe their grade is 1.8 gpt gold and 180 gpt silver? In that ballpark, anyway.
The wiki page on gold cyanidation has further information.
Now, as to exact economics, each project is different. For example, if there's any zinc in the ore, you have what's called an interfering element, because zinc has greater affinity for the cyanide than does gold. You have to watch the acidity of the solution (pH), so sulphides in the ore can cause problems. And so on. I did a broad search, and it looks like typical cyanide consumption lies in the range of 300-500 grams cyanide for each gram of gold recovered. Based on the typical price for cyanide, call it a buck's worth per gram of gold. There are often other chemical inputs involved, but I'm trying to keep it simple.
Often, you'll see cyanide leach combined with other gold recovery methods. An example was put forward of 10 gpt gold. They'd probably use a gravity/density recovery method to extract the larger gold particles (which coincidentally dissolve more slowly, as solvation is a surface phenomenon), prior to submitting the gravity tailings to cyanidation. Or, if there was a mixed sulphide/oxide deposit, perhaps a flotation circuit to isolate the sulphides prior to cyanidation would be in the mix.
Unfortunately, there is no standard or ideal mine to consider. Unique variables always influence the optimal extraction method, and thus, the costs.
Lar