Skip to content
Sign in

Post

Silver Falcon Mining

You’re reading Silver ion’s reply in this thread.Jump to it

Prez3.9 rating from 73 members9.8K ptsRate

Couple of points...

Nice update, and good news on the permit.

Sounds like they need more work on the Sinker. An earlier PR had mentioned how far rock bolting had advanced, which was obviously not nearly the whole length. There was some speculation that maybe it had only been bolted as far as the targets identifed by RS. But it appears more bolting is required. That will take a while, depending on how much more they have to do. A good question for the SHM.

Also, as I've pointed out a few times, once they get the flotation system in, and start redoing the 30k tons of previously processed ore, it will mean not being able to process new ore during that time. Since they won't be bringing any new ore down for the winter, they obviously think it will take at least until next spring, maybe longer to reprocess the ore. Remember it took two years to process that amount the first time. Hopefully this will go faster than the original processing since the ore is already ground pretty well. But it also means that they will be running partially depleted stuff (~4g/t?) with ~20% of the gold removed rather than the original (~5g/t?). Maybe less time will be required and make up for the lower grade.

Join the conversation about Silver Falcon Mining.

Reply

Replies

  1. " But it also means that they will be running partially depleted stuff (~4g/t?) with ~20% of the gold removed rather than the original (~5g/t?). Maybe less time will be required and make up for the lower grade."

    Hi Spiny,

    So if my math is right, we should get another 20 to 25 grams per ton from the ore because only 15 to 25% was processed in the first place. Processing the ore again won't give as much yeild as processed new ore, but it might be more effecient and less expensive to do it this way, instead having to load and trucking new ore down the mountain. Besides that, pulling another 20 t0 25 grams of concentrate out of the ore isn't chicken feed and if it can be procecced faster than the first time thru, that could be another plus. JMHO

    Go SFMI/GHDC

    1. Silver Ion-

      My original numbers were correct. The assays you see for the mill feed are the real gold content, averaging around 5 g/t. At the 20% mill efficiency, they remove about ~1 g/t leaving ~4 g/t. Do the math on the value they are quoting for the 30k tons and you'll see. 30k tons at 4 g/t is about 4000 oz, which at $1600 gold is ~$6.4M, about what they are claiming. So that 30k tons of partially depleted ore is about 4g/t, not 20. Processing this ore will certainly save by not having to truck new ore, and should process faster since it is already milled to a fairly small size (though I get the impression it requires more milling). There's a good chance that the savings will make up for the fact that this ore has already had ~20% of the gold removed. But the ore does not contain anywhere near 20g/t.

      1. Spiny...

        My mistake was thinking that 4 g/t gold was extracted already, not 1 g/t gold. So I was using 4 to 5 grams from the assays as the base numbers to multiply into 20 to 25 g/t.

        Thanks for your reply.

        Go SFMI/GHDC

    1. Macod- I realize itwill be a while until the leaching system is in. But it was my impression that the flotation system that is presumably ready to install will also increase the recovery.